When a silicone compound comes out too soft, too brittle, or impossible to process, the review usually starts with the crosslinker or the filler. More often, the root decision was made one step earlier: the choice of the vinyl silicone oil used as the base.

Two numbers decide — and they answer different questions.

  1. Vinyl content sets the cure. It is the vinyl groups that react with Si–H under platinum catalysis, so vinyl content determines crosslink density: higher vinyl content → harder, stronger, more tear-resistant networks; lower vinyl content → softer, more extensible networks. A compound that cures brittle or undercures soft usually has the wrong vinyl grade, not the wrong catalyst.
  2. Viscosity sets the process. Viscosity decides how much filler the base can carry, how the compound flows, and whether it can be injected. Low-viscosity grades accept high filler loading and feed LSR injection lines; high-viscosity grades build green strength and final tear resistance in HTV.

IOTA 273 is vinyl-terminated polydimethylsiloxane (CAS 68083-19-2) covering both axes in one product family:

Viscosity (25°C, mPa·s) Molecular weight Vinyl content (%) Density (g/cm³)
0.7 186 29 0.81
2-3 500 10-12 0.92
4-6 770 7-9 0.93
10 1000 5.4 0.95
20 2000 2.7 0.95
100 6000 0.8-1.2 0.97
200 9400 0.4-0.6 0.97
500 17200 0.37-0.43 0.97
1000 28000 0.18-0.26 0.97
3500 43000 0.12-0.15 0.97
5000 49500 0.10-0.13 0.97
10000 62700 0.08-0.12 0.97
20000 72000 0.06-0.09 0.98
65000 117000 0.04-0.06 0.98
165000 155000 0.03-0.04 0.98

Where it is used:

  1. HTV base raw material — raises hardness and strength of high-temperature vulcanized silicone rubber.
  2. LSR main material — the base polymer of injection-molding liquid silicone rubber, where low viscosity plus controlled vinyl content feeds fast-cycling molds.
  3. Modification of organics — reacts into polyurethane and acrylic systems (10-20% dosage) to add weathering, ageing and UV resistance with reinforcement and toughening; dosage as base gum is 50-100%.

Packaging: 50 kg or 200 kg drums. Store sealed, dry and shaded at room temperature, away from fire and direct sun, and away from impurities — especially catalysts and acidic substances. Non-dangerous goods.

If your compound review keeps circling back to "soft but weak" or "hard but brittle," start the next trial from the vinyl content of the base — IOTA 273 has a grade for each point on the curve.